Alloy Steel Welding Techniques

Alloy Steel Welding Techniques Points : Alloy Steel Welding Techniques Thicker part is ready by the common 90° V with the surfaces clean of all impurity. Welding is perform in the leftward way and the flame is play above a large area than common as of the low thermal conductivity.This lessons the risk of melting a hole in the sheet. Tip of the internal cone is kept extremely secure to the surface of molten pool with the welding perform accurately as for the leftward welding of mild steel. No paddling must be done and the least feasible quantity of blowpipe motion use. After welding martens tic stainless steel should be heated to 700°C to 800°C and then gone to air cool. Non- stabilized steels need heat treatment after welding if they are to encounter corrosive situation or else no heat treatment is required.